Looking for durable and high-performance stainless steel plates? Our 446 BA stainless steel plates offer exceptional resistance to high temperatures and oxidation, making them ideal for industries that demand reliability and strength. These plates are widely used in applications such as , exposed to elevated temperatures.

 

GNEE offers 446 stainless steel plate, treated through a bright annealing (BA) process to achieve a smooth, highly reflective matte finish. It can withstand temperatures up to 816℃. Available in thicknesses from 0.5 to 12 mm and widths from 1500 to 2000 mm (custom sizes available), it is suitable for high-temperature furnace components, automotive exhaust systems, heat exchange equipment, and chemical corrosion-resistant parts. GNEE also provides original quality inspection reports and fast delivery.

 

446 BA Stainless Steel plate

: 446 BA Stainless Steel

: 0.5mm – 100mm (custom sizes available)

: 1000mm – 2000mm (custom widths available)

: ASTM A240, A480

: High-temperature environments, heat exchangers, furnace parts, industrial machinery

sales@gneestainless.com

 

% Weight (446)
<=0.30
1.00-2.00
<=0.04
<=0.02
0.75-1.50
23.0-27.0
0.25-1.00
<=0.20

 

: >=520 MPa

: >=205 MPa

: >=25%

: <= 90 HRB

 

 

446 stainless steel plates are processed using advanced production equipment to ensure the precision and consistency of each plate. The factory utilizes efficient tools such as laser cutting machines, CNC punching machines, and polishing equipment, capable of processing a wide range of stainless steel plate thicknesses from 0.3mm to 8mm, ensuring that products meet international standards such as ASTM A240. Before shipment, each batch undergoes rigorous quality inspections, including surface finish, thickness tolerance, and dimensional accuracy, to ensure that the product meets customer requirements.
After bundling, the products are packaged with waterproof paper and wooden pallets. This secure packaging prevents damage during transportation and can be customized to meet regulatory and customer requirements. In addition, each product packaging is clearly labeled for easy identification and quality information.